Lincoln TG55125638 Techalloy 55 TIG (GTAW) Rod, 1/8 in, (3) 10 lb Tube
TECHALLOY 55 is ideal for a preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks.Features
• The welds are moderately hard and require carbide tipped tools for machining• A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks
• Q2 Lot certificates showing actual wire composition available online
•
Lincoln TG55125638 Techalloy 55 TIG (GTAW) Rod, 1/8 in, (3) 10 lb Tube
TECHALLOY 55 is ideal for a preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks.Features
• The welds are moderately hard and require carbide tipped tools for machining• A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks
• Q2 Lot certificates showing actual wire composition available online
•