Lincoln ED019888 Lincore 60-O Flux-Cored (FCAW-S) Wire, 7/64 in, 50 lb Coil
LINCORE 60-O Flux-Cored Wire typical application on Bucket lips, Crusher hammers, Ore chutes, Dozer blades and Ripper teeth deposits feature higher alloy levels than to resist both abrasion and moderate impact. Can be used at temperatures up to 704°C (1300°F) Deposit thickness limit is two layers unless high travel speed is used to obtain very closely spaced check cracks. Many layers can be used with high travel speed and small bead sizes to ensure close-spaced check cracks. Lincore 60-0 deposit cross cracks (commonly called cross-checking) on cooling. This is desirable, since cross-cracking of the deposit relieves cooling stresses and prevents spalling.Features
• Deposits feature higher alloy levels than to resist both abrasion and moderate impact• Can be used at temperatures up to 704°C (1300°F)
• To be used on carbon, low alloy, manganese, stainless steels and cast iron
• Deposit is limited to two layers
Lincoln ED019888 Lincore 60-O Flux-Cored (FCAW-S) Wire, 7/64 in, 50 lb Coil
LINCORE 60-O Flux-Cored Wire typical application on Bucket lips, Crusher hammers, Ore chutes, Dozer blades and Ripper teeth deposits feature higher alloy levels than to resist both abrasion and moderate impact. Can be used at temperatures up to 704°C (1300°F) Deposit thickness limit is two layers unless high travel speed is used to obtain very closely spaced check cracks. Many layers can be used with high travel speed and small bead sizes to ensure close-spaced check cracks. Lincore 60-0 deposit cross cracks (commonly called cross-checking) on cooling. This is desirable, since cross-cracking of the deposit relieves cooling stresses and prevents spalling.Features
• Deposits feature higher alloy levels than to resist both abrasion and moderate impact• Can be used at temperatures up to 704°C (1300°F)
• To be used on carbon, low alloy, manganese, stainless steels and cast iron
• Deposit is limited to two layers