Lincoln TG99093638 Techalloy 99 TIG GTAW Welding Rod, 3/32 in, 10 lb Tube
TECHALLOY 99 is ideal for a preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks. Welds produced are generally more machinable than a Tech-Rod 55 deposit.
Features
• Welds produced are generally more machinable than a Tech-Rod 55 deposit
• A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks
• Q2 Lot certificates showing actual wire composition available online
•
Lincoln TG99093638 Techalloy 99 TIG GTAW Welding Rod, 3/32 in, 10 lb Tube
TECHALLOY 99 is ideal for a preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks. Welds produced are generally more machinable than a Tech-Rod 55 deposit.
Features
• Welds produced are generally more machinable than a Tech-Rod 55 deposit
• A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks
• Q2 Lot certificates showing actual wire composition available online
•